Also wanted to see how much darker a shorter exposure would be.
Here are all the images in order of printing. (number and info is below each image)

image #3 from KM photopolymer plate from Takach Press
10' stocastic screen aquatint exposure and 10' image exposure

image #5 from KM photopolymer plate from Takach Press
10' stocastic screen aquatint exposure and 8' image exposure

image #7 from KM photopolymer plate from Takach Press
10' stocastic screen aquatint exposure and 6' image exposure

image #9 from KM73 photopolymer plate from Boxcar Press
10' stocastic screen aquatint exposure and 10' image exposure

image #11 from KM73 photopolymer plate from Boxcar Press
10' stocastic screen aquatint exposure and 8' image exposure

image #13 from KM73 photopolymer plate from Boxcar Press
10' stocastic screen aquatint exposure and 6' image exposure

image #15 from KM73 photopolymer plate from Boxcar Press
10' stocastic screen aquatint exposure and 5' image exposure